When processing plastic enclosures, it is essential that the tools be cooled only using oil-free air. Drilling, cooling and lubricating methods can all lead to stress cracks.
If silicone-based lubricants are used, then a downstream printing process is not possible due to the poor adhesive properties of the lacquer. If cases of doubt, we would be pleased to provide specific information.
When working with our milling machines and planning to make openings, you are advised to apply a general radius of 1.5 mm.
NB: Our processing service excludes any such risks.
When punching out plastic parts, crack formation and stress whitening at the corners can never be ruled out. The BOPLA processing service minimizes any such risk.
The quality of any adhesive connection depends on the materials being glued, the size of the area to be glued and the glue itself.
Make sure to observe the following ...